Abstract
Most hulls of the ships are protected with paintings, sacrificial anode, and impressed current cathodic protection methods against corrosion problems. However, these conventional methods are not very effective because the rudder of ships stern are exposed to very severe corrosive environment such as tides, speeds of ships, cavitations and erosion corrosion. The environmental factors such as cavitation and corrosion will cause damage for materials with the shock wave by the creation and destruction of bubble. To solve these problems, the cavitation and electrochemical experiments are executed for thermal spray coating with Al–Zn alloy wire material. Thereafter, and sealed specimens with F–Si sealer on Al–Zn alloy coated specimen are executed to improve electrochemical and anti-cavitation characteristics in sea water. The application of fluorine silicon sealing after spray coating of 15%Al–85%Zn seems to be appropriate not only in static environment but also in dynamic environment.

Key words
cavitation; Al–Zn alloy wire material; thermal spray coating; corrosion

 

本站文章未经允许不得转载;如欲转载请注明出处,北京桑尧科技开发有限公司网址:http://en.sunspraying.com/

Support
返回首页
Home page
发表评论 共有条评论
用户名: 密码:
验证码: 匿名发表
Information
Article
    无相关信息
Update
Hot